You spot a dent, a crack or a dull patch on a carbon fibre panel. Your first instinct is probably to grab the abrasive and start tidying it up. Hold off. We have watched more than one good panel get ruined because someone rushed to patch what they could see. On a composite structure, the surface almost always hides more than it shows, and that gap between visible and actual damage is where most repair problems begin. Repairing carbon fibre composite damage on aircraft starts with patience, not tools.
Picture a composite laminate as a stack of fibre sheets bonded together by resin. When that bond fails somewhere inside the stack, the layers begin to separate. Engineers call this delamination. The outer skin can look perfectly clean while the interior slowly loses its load capacity. That is exactly why assessment has to come before any work begins on the panel. We have seen teams treat a clean-looking surface as a clean-looking structure, and it cost them weeks later.
Assess First, Then Choose the Method
The sequence we follow on the shop floor is deliberately simple. The first step is confirming how far the damage really extends, using a tap test followed by ultrasonic C-scan. The second step is selecting a scarf or bolted repair that stays within the limits of the Structural Repair Manual (SRM). Skipping the first step is the most common reason repairs get rejected later. It is also the mistake we see most often from newer teams, who want to start cutting before they know the boundary.
Assessment is not a formality. It sets the size of the repair, the materials you order and the time the aircraft stays on the ground. A rough estimate made from the visible mark will almost always be too small.
Reading What the Symptoms Tell You
Most jobs start with something small. A ground vehicle clips a fairing, a tool slips across a skin, or hail leaves a row of marks along a leading edge. Each symptom points toward a different kind of problem, and reading it correctly saves hours downstream.
Dents, crushed fibres and cracked paint after a handling incident are the obvious signs. Cracked paint can look like a cosmetic issue, but it often means the laminate beneath experienced a load it was never designed to carry. A hollow or dull sound when you tap the surface is more serious. It usually points to delamination.
Hail, bird strikes and runway debris leave impact damage that tends to run deeper than the surface suggests. Discolouration around fasteners or edges after heat or lightning exposure means you need to think about conductivity and heat paths. The outer finish alone will not tell you that, so do not rely on it.
Mapping the Damage with Tap Test and Ultrasonic Inspection
Before any sanding, mark the damage boundary and transfer it to a drawing. This may feel like paperwork. It is also what lets you justify your repair decision later. Auditors will ask for exactly this record, and they are right to expect it.
The tap test is quick. A technician taps the surface with a coin or a light tapping tool and listens closely. Solid laminate rings sharp, while a delaminated area sounds flat or hollow. It works well for screening, but it cannot tell you depth. For that you need ultrasonic inspection, either pulse-echo or through-transmission. It reads the internal layers and reveals the real extent. In our experience, the ultrasonic map is often considerably larger than the zone the tap test flagged.
Record everything: the tap-test result, the ultrasonic image, the measurements and the date. A repair decision that cannot be traced back to evidence is a repair that will be questioned.
Scarf or Bolted: Matching the Method to the Damage
There are two main ways to restore a composite structure. A scarf repair removes material in a long, gentle taper and bonds new plies into the opening. It keeps the aerodynamic surface smooth and carries load well, which is why it suits thinner laminates and moderate structural damage.
A bolted repair uses mechanical fasteners and doubler plates. It becomes the practical choice when access is limited or the damage is large, since you do not have to remove as much sound material. The trade-off is added weight, plus fastener holes that need their own inspection schedule afterwards. Load paths, weight and inspection access should all be weighed before committing to a method. The right choice is the one the SRM and the engineering disposition allow, not simply the faster one.
Wet Layup or Prepreg
Wet layup means dry fibre is saturated with resin on site. It is flexible and works well on complex contours and in the field. The resin-to-fibre ratio is harder to hold steady, though, so it demands real discipline from the technician.
Prepreg arrives with a measured amount of resin already impregnated. Fibre volume and properties are more consistent, which is why it is usually preferred for primary structure, provided you have the cure equipment. Whichever you choose, match fibre orientation, ply count and resin system to the original laminate specification. A repair that is stronger in one direction than the parent part is just as wrong as one that is weaker.
Keeping the Cure Under Control
A large share of the final strength in a composite repair is set during cure. The ramp rates and dwell times in the repair documentation are not suggestions. Straying from them can leave the resin under-cured or leave voids that weaken the bond line.
Vacuum bagging with breather and bleeder plies removes trapped air and keeps void content under control. Thermocouples placed directly on the repair confirm the actual temperature rather than trusting the oven set point. And log every cycle, because traceability is part of the repair itself.
Staying Inside SRM Limits
Before you start, check the damage size, location and type against the SRM allowable damage limits. This is the step people tend to skip when the damage looks minor. If it falls outside those limits, the decision belongs to engineering, however experienced the technician is. Reference the applicable maintenance task in the repair record so anyone reading it later can follow the logic from assessment to sign-off. For wider context on how these structures are kept airworthy, our team also covers aircraft maintenance practice in more depth.
A Ground-Damage Case From Our Own Floor
A ground-service vehicle once struck a composite fairing and left a dent with suspected delamination. The tap test flagged a hollow zone around the impact point. The ultrasonic scan then showed the delaminated area was roughly three times the size of the visible mark. That single measurement changed the whole plan.
We went with a scarf repair using prepreg, cured under vacuum, and re-inspected after the cure. The lesson stuck with the whole team: the visible dent was the smallest part of the problem. If you want background on how these laminates behave under load before you start, our overview of carbon fibre reinforced polymers in aerospace is a good starting point.
Common Mistakes That Lead to Rejection
Most rejected repairs trace back to a handful of habits. Skipping ultrasonic inspection is the big one, because it leads to underestimating how far the delamination runs. Wrong ply orientation or fibre volume weakens a repair even when it looks flawless. Poor surface preparation leaves contaminants at the bond line, and a bond that fails there cannot be seen from outside. Curing outside the specified temperature and pressure window is the last common trap, and it is almost impossible to correct afterwards.
Frequently Asked Questions
Can carbon fibre damage be repaired without removing the part from the aircraft?
Sometimes. Many small, accessible repairs are done in place, provided the SRM allows it and you can reach the area for proper inspection and cure control. Larger or deeper damage usually requires removing the part.
How do I know whether a repair needs a scarf or a bolted approach?
Look at laminate thickness, damage size, access and load path. Thinner laminates with moderate damage usually suit a scarf, while limited access or larger damage often points to bolted. The final call should follow the SRM and engineering disposition.
Is a tap test enough to rule out internal damage?
No. It is a screening tool and can miss depth. Confirm the real extent with ultrasonic inspection before you decide anything.
Who must approve a repair that falls outside SRM limits?
Engineering must approve it through a formal disposition. The shop should never make that call alone.
If you are facing damage on your own fleet, start with the assessment and do not skip the ultrasonic map. For material and supply questions beyond the shop floor, you can also check monapay.vn.